Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.61 kN/m | 9.20 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N5000-30/32 BT Epoxy Package The Nelco N5000-30 prepreg and N5000-32 laminate BT epoxy materials are designed specifically to meet or exceed new and emerging chippackaging requirements. The primary applications of these materia.. |
|||
Peel Strength | 1.61 kN/m | 9.20 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-12 SI® High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |
|||
Peel Strength | 1.61 kN/m | 9.20 pli | To Copper (1 oz./35 micron); After Process Solutions; IPC TM-650 2.4.8 |
Arlon 37N Polyimide Low-Flow 37N is a polyimide low-flow prepreg suitable for bonding multilayer polyimide rigid-flex, attaching heat sinks to polyimide MLBs, or other applications where minimal and uniform resin flow is requir.. |
|||
Peel Strength | 1.61 kN/m | 9.20 pli | Bond Strength; ASTM D624 |
Arlon 51576XC015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Cured Silicone Rubber This data represents typical values for the production mat.. |
|||
Peel Strength | 1.61 kN/m | 9.20 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Peel Strength | 1.61 kN/m | 9.20 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep.. |
|||
Peel Strength | 1.61 kN/m | 9.20 pli | after solder float; IPC-TM-650.2.4.8 |
Park Electrochemical Nelco® N4000-12 High Speed/Low Loss, CAF Resistant Laminate and Prepreg The Nelco® N4000-12 series is an enhanced epoxy resin system designed for use in high speed, low loss applications requiring thermal stability, excellent signal speed and CAF resistance.Key Feature.. |