Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.38 kN/m @Temperature 288 °C, Time 20.0 sec |
7.90 pli @Temperature 550 °F, Time 0.00556 hour |
IPC-TM-650 2.4.8 |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | (S1 to S2) Bond Strength |
Arlon 56810R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 1564 Style Fiberglass This data represents typical values for the production material. The data should not be.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 8620 ES Conformable Graphic Film These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 8620Cv2 ES Changeable Graphic Film with Comply™ v2 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | (S2 to S2), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55106R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silic.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | (S2 to S2), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55146R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red sili.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | (S1 to S1), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55149R028 0.0295" (0.749 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | (S1 to S2), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55276R026 0.026" (0.660 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red si.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 8620Cv3 ES Changeable Graphic Film with Comply™ v3 Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | Adhesion to Aluminum, anodized |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Peel Strength | 1.38 kN/m | 7.90 pli | (S2 to S2), Bond Strength; Arlon SQA-TMS-011 |
Arlon 55276R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone Rubber Substrate: Style 162 FiberglassSide 1: Cured Silicone RubberProduct Use: Flexible heater insulationAppearance: Red silic.. |