Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.66833 kN/m | 3.8125 pli | to Polyester, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 444PC Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 468MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Smooth Powder Coating, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9472 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 9668MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polypropylene, 90° peel, 12"/min, 2 mil aluminum, 72 hr at 70°C; ASTM D3330 |
3M 9674 Adhesive Transfer Tapes with Adhesive 300 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 300 offer excellent adhesion to a wide variety of surfaces, including low surface energy plastics and foam. This pressure sensitive acrylic adhesive f.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7880HL Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated white polyester facestock with 0.8 mil acrylic adhesive 300 on a 78 lb clay-coated kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abras.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polypropylene, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7904 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Material 7904 is a durable, high performance material that offers excellent conformability, good durability and moisture resistance. This label material utili.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | to stainless steel, 90°, 72 hr RT; ASTM D3330 |
3M 9009 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | to Polycarbonate, 90°, 2 mil al foil, 72 hr RT; ASTM D3330 |
3M 9009 Double Coated Tapes with Adhesive 300 3M™ Double Coated Tapes with 3M™ Adhesive 300 feature a thin polyester film for dimensional stability and improved handling with ease of die cutting and laminating. The high tack adhesive provides.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | ABS, 90° Peel, 72 hr dwell; ASTM D3330 |
3M 9018FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 9017FL and 9018FL are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. T.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 90° Peel, PET/PET, 72 hrs at RT; ASTM D3330 |
3M 9061MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 9185MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 467MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 468MPF High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 7955MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | 72 hour RT acrylic, 90° peel, 2 mil aluminum foil backing |
3M 7965MP High Performance Adhesive Transfer Tapes with Adhesive 200MP 3M™ High Performance Acrylic Adhesive 200MP is a popular choice for graphic attachment and membrane switch applications because it has excellent quality, consistency and durability. In addition, as.. |
|||
Peel Strength | 0.66833 kN/m | 3.8125 pli | Polycarbonate 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |