Polymer Property : Peel Strength = 0.631 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.631 kN/m

@Temperature 85.0 °C,
Time 605000 sec
3.60 pli

@Temperature 185 °F,
Time 168 hour
ASTM D1000
Parker Chomerics CHO-FOIL CCH Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..
Peel Strength 0.631 kN/m

@Temperature 121 °C,
Time 605000 sec
3.60 pli

@Temperature 250 °F,
Time 168 hour
ASTM D1000
Parker Chomerics CHO-FOIL CCH Shielding Tape
Conductive Adhesive Copper FoilDescription: Chomerics’ CHO-FOIL® tapes are an economical EMI shielding solution for a variety of commercial uses. The tapes are available in copper, aluminum, or ti..
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; MIL-I-46852C
Arlon HS930-10R##-P4 0.030" (0.762 mm) Self-Fusing Silicone Tape (Rectangular, Unsupported)
Description: High Strength, 1 inch wide, 30 mil thick, Red, Rectangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicat..
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; MIL-I-46852C
Arlon LW401B##-P1 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; MIL-I-46852C
Arlon LW401B##-P2 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; MIL-I-46852C
Arlon P3272-10Rxx-P4 0.030" (0.762 mm) Cured Self-Fusing Silicone Tape (Rectangular, Unsupported)
Description: High strength self-fusing silicone tapeDesign/Construction: Interleave: PolyethyleneRubber: Cured Self-Fusing Silicone Rubber Cross-Section: 1” wide RectangularAppearance: Red silicone..
Peel Strength 0.631 kN/m
3.60 pli
ABS Plastic, 180°, after 48 hrs at 23°C
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives
3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; Arlon SQA-TMS-011
Arlon 54331R014 0.014" Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Blue LDPESide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Blue LDPEThis data represents typical valu..
Peel Strength 0.631 kN/m
3.60 pli
Bond Strength; MIL-I-46852C
Arlon LW401B##-P0 0.040" (1.02 mm) Cured Self-Fusing Silicone Tape (Triangular, Unsupported)
Description: 1 inch wide, 40 mil thick, Black, Triangular cross-section, Self-Fusing Silicone Tape. Product is supplied in various roll lengths and the ## in the product number indicates roll length..
Peel Strength 0.631 kN/m

@Temperature -55.0 °C
3.60 pli

@Temperature -67.0 °F
Aluminum, etched, Bell Peel, Cohesive Failure; ASTM D3167
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives
3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f..