Polymer Property : Peel Strength = 0.62451 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.62451 kN/m
3.5625 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7002 Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.62451 kN/m
3.5625 pli
LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7002FP Performance Paper Label Material
3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne..
Peel Strength 0.62451 kN/m
3.5625 pli
Polycarbonate 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330
3M 7907 Screen Printable Sheet Polyester Label Material
3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat..
Peel Strength 0.62451 kN/m
3.5625 pli
90° Peel, PET/Polycarbonate, 72 hrs at RT; ASTM D3330
3M 7951 Hi-Performance Acrylic 300MP
This adhesive is designed for applications requiring greater initial adhesion especially to low surface energy (LSE) plastic substrates. Temperature performance is up to 300°F (149°C) for most app..