Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.596 kN/m | 3.40 pli | Bond Strength; Arlon- SQA-TMS-015 |
Arlon 920-410C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
(discontinued **) Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Peel Strength | 0.596 kN/m | 3.40 pli | Bond Strength; Arlon- SQA-TMS-015 |
Arlon 920-05C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 0.5” Wide Rectangular .0.5 inch wide, 20 mil thick, Black, Rectangular cross-section, Se.. |
|||
Peel Strength | 0.596 kN/m | 3.40 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon 920-10CxxFR-P1 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, brown, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Peel Strength | 0.596 kN/m | 3.40 pli | Bond Strength; MIL-I-46852C |
Arlon 930-10Bxx-P0 0.030" (0.762 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 30 mil thick, Black, Rectangular cross-section, Self-fu.. |
|||
Peel Strength | 0.596 kN/m | 3.40 pli | PVC, 180°, after 48 hrs at 23°C |
3M Fastbond™ 4224-NF Pressure Sensitive Adhesives 3M™ Fastbond™ Pressure Sensitive Adhesive 4224-NF is a water-based, permanently pressure sensitive adhesive with excellent initial tack and good bond strength.Information provided by 3M |
|||
Peel Strength | 0.596 kN/m | 3.40 pli | Bond Strength; ASTM D624 |
Arlon R34591R014 0.014" (0.356 mm) Uncured Silicone Rubber Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 2116 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicon.. |
|||
Peel Strength | 0.596 kN/m | 3.40 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon T1020-R004-## 0.020" Self-Fusing Silicone Rubber Tape 1 inch wide, 20 mil thick, red, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number.Desi.. |