Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.5478 kN/m | 3.125 pli | Rubber, Adhesion; ASTM D3330 |
3M 411DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | HD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7002 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Polyester, 180° Peel, Initial 10 min dwell at RT; ASTM D3330 |
3M 7743FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7743FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films utilize a clear or matte polyester film that is recommended for optimum durability and outdoor UV exposure. 3M™ Adhesive 400 offers excellent low temperature per.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Steel, 180° Peel, 72 hr dwell, Faceside; ASTM D3330 |
3M 9416 Repositionable Tape 3M™ Repositionable Tapes are double coated tapes that are ideal for applications where one or both parts need to be repositioned or removed easily.Information provided by 3M |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Non-linered side-Urethane-B, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1920S Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Non-linered side-Urethane-A, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1120 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M Scotch® 373 High Performance Box Sealing Tape Scotch® Box Sealing Tape 373 is a performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a heavy duty, conformable backi.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | HD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7905 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7931 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7983 Sheet Polyester Label Material Features:Matte coating is compatible with screen printing and resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations. Variable information can be added by the end .. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Aluminum, 180° peel, 72°F, (72 hr. dwell); ASTM D3330 |
3M 9442 Adhesive Transfer Tapes with Adhesive 350 These 3M™ Adhesive Transfer Tapes with 3M™ Adhesive 350 are a modified acrylic adhesive ideal for very high-bond strength to many surfaces. They have excellent chemical resistance and bold strengt.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | LDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9628FL Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Non-linered side-Composite Sleeve, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1060 Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1920S Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel |
3M Scotch® 8484 Combining Tape Scotch® Combining Tape 8484 is a systems length polypropylene combining tape with a serrated edge.Information provided by 3M |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Steel; ASTM D3330 |
3M ScotchPad™ 830CP Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Glass, 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7744 Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Glass, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Adhesion to Housewrap; ASTM D3330 |
3M 8067 All Weather Flashing Tape 3M™ All Weather Flashing Tape 8067 is a self-adhered, waterproof flashing membrane designed for sealing around openings and penetrations in exterior walls. This product has a unique acrylic pressur.. |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | LDPE, 180°, 2 mil al foil, 72 hr RT, Faceside; ASTM D3330 |
3M 9628B Double Coated Tape with Quick Bonding Adhesive 360 3M™ Double Coated Tapes with 3M™ Quick Bonding Adhesive 360 provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and powder coated paints... |
|||
Peel Strength | 0.5478 kN/m | 3.125 pli | Non-linered side-Polyester, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1920 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |