Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 0.526 kN/m | >= 3.00 pli | Silicone Aluminum; Cured; ASTM D1876 |
Parker Chomerics Tecknit TeckBond™-NC Nickel Coated Graphite-Filled Adhesive Description: TECKBOND-NC is a silicone rubber base filled with nickel coated graphite particles to produce a highly conductive one-component adhesive sealant. The system is an RTV moisture-cured com.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Polypropylene, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7041 Screen Printable Polyester Performance Label Products 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer good thermal stability and moisture resistance. These topcoated polyester label stocks u.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | (S1 to S2), Bond Strength; Arlon-SQA-TMS-011 |
Arlon 51366X015 0.016" (0.406 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Flame Resistance: Product is designed to meet Title 14 CFR.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Cold Rolled Steel, 180°, after 48 hrs at 23°C |
3M Fastbond™ 49 Insulation Adhesive 3M™ Fastbond™ Insulation Adhesive 49 is a water-based, high solids, fast tacking, pressure sensitive adhesive for bonding lightweight materials like fiberglass insulation, felt, shoddy, paper and .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM061 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM128 Indoor UL Recognized White Polyester Label Products 3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM16J Indoor UL Recognized Computer Imprintable White Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FMV02 Void Polyester Label Products 3M™ Void Polyester Label Products are tamper-indicating stocks designed to provide a “void” message in the facestock when removal is attempted. These void polyester labels utilize 3M™ Adhesive P.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV095 Soft Translucent Vinyl Label Products 3M™ Soft Translucent Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV362 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Glass |
3M Scotchcal™ 50-914 Graphic Film Film series 50 is a 3-mil calendered vinyl film, available in 28 colors. The film has a clear, pressure-sensitive film with a blue liner on the white films for easier visibility when wedding, and a .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7125-13 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7125-24 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to FRP |
3M Scotchlite™ 680-81 Reflective Graphic Film 7-mil, enclosed lens, retroflective, engineer grade films that offer flexibility and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appear.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | LD Polypropylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 90°, Adhesion to Polypropylene |
3M Bumpon™ SJ5916 Resilient Rollstock 3M Bumpon Resilient Rollstock Products are opaque, colored polyurethane materials produced with aggressive pressure-sensitive adhesives.Information provided by 3M |
|||
Peel Strength | 0.526 - 0.877 kN/m | 3.00 - 5.00 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ IJ180Cv3-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FL01000N Lexan Label Product 3M™ Lexan Label Products are durable, matte clear polycarbonate overlaminates that offer excellent moisture and abrasion resistance. These lexan labels utilize 3M™ Adhesive P1212, which is a high .. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM14K Indoor UL Recognized Computer Imprintable Clear Polyester Label Product 3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM239 Indoor UL Recognized Matte Clear Polyester Label Products 3M™ Indoor UL Recognized Matte Clear Polyester Label Products FM23N, FM232 and FM239 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These po.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP011 Clear Polypropylene Label Products 3M™ Clear Polypropylene Label Products are biaxially oriented film materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV032R Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7125-64 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7725-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Adhesion to Polypropylene |
3M Scotchcal™ ElectroCut™ 7725-85 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | Glass, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7980 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.526 kN/m | 3.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM03K Indoor UL Recognized Clear Polyester Label Products on 3M™ Indoor UL Recognized Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products are suitable for dem.. |
|||
Peel Strength | >= 0.526 kN/m | >= 3.00 pli | [ppi], Bond Strength |
Arlon 42561R006 0.0055" (0.140 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Rubber Side 2: RubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specificationsInforma.. |