Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.351 - 7.89 kN/m | 2.00 - 45.0 pli | Average value: 3.49 kN/m Grade Count:13 |
Overview of materials for Epoxy Encapsulant, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Encapsulant, Unreinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HDPE, 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M 7026 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Stainless Steel, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7744FL Polyester Overlaminating Film 3M™ Polyester Overlaminating Films 7744 and 7744FL utilize a matte clear polyester that is recommended for optimum durability and thermal transfer printability. 3M™ Adhesive 400 offers excellent l.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | LD Polyethylene, 180° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Adhesion to Aluminum, steel, stainless steel, titanium, zinc, cadmium, chromium, magnesium, glass, enamel, Epoxy MIL-P-23377 and Urethane MIL-C-27725 |
3M AC-215 Class B-2 Aerospace Sealant 3M Aerospace Sealant AC-215 Class B are two-part, polysulfide access door sealants for faying surfaces where easy separation of jointed surfaces is required. They are a highly thixotropic reddish pa.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Bond Strength; Arlon SQA-TMS-015 |
Arlon 910-10Rxx-P1 0.010" Cured, Self-Fusing Silicone Rubber 1.0 inch wide, 0.010" thick, red, rectangular cross-section, silicone self-fusing tape. Product is supplied in various yard long roll lengths as indicated by the xx characters in the part number.De.. |
|||
Peel Strength | >= 0.351 kN/m | >= 2.00 pli | Government Bond |
Arlon LW5015Rxx-P1 0.050" (1.27 mm) Self-Fusing Silicone Tape (Triangular, Unsupported) with Poly Interleave Design/Construction: Triangular Cross Section Fusible TapeArlon LevelWrap® Tape: LevelWrap® has tapered edges and a colored line along its apes. The purpose of the line is to act as a guide for su.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV1172 Removable White Vinyl Label Products 3M™ Removable White Vinyl Label Products FV1172 and FV392 are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive .. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Polycarbonate 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | LD Polyethylene, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7903 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7903FL Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | HD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7925 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM0196J MC Polyester Label Product 3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV022902 Soft White Vinyl Label Product 3M™ Soft White Vinyl Label Product FV22902 is a flexible vinyl label stock that offers excellent durability and some moisture resistance. This vinyl label utilizes 3M™ Adhesive F2201 which is a fr.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV1002 Soft White Vinyl EDP Label Product 3M™ Soft White Vinyl EDP Label Products FV100K and FV1002 are flexible vinyl label stocks that offer excellent durability and some moisture resistance. These vinyl labels utilize 3M™ Adhesive F220.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° Peel 12"/min, 1" wide sample; TLMI Method |
3M P1500 Medical Permanent Acrylic Adhesives 3M™ Medical Permanent Acrylic Adhesives P1500 demonstrates excellent peel and tack performance and are designed for use in the medical attachment market.Information provided by 3M |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 180° |
3M Scotch-Weld™ DP-105 Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP105 Clear is a fast setting, very flexible 1:1 mix ratio epoxy adhesive/sealant. Its flexibility when cured makes it ideal for applications involving dissimilar s.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Stainless Steel, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7884 White Vinyl Label Material Features:Conformable to contoured surfacesResists wrinkling and delaminationOne-piece removal up to one year after applicationTopcoated for impact printing, typewriters, ballpoint pens, pencils, and.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7902 Screen Printable Sheet Vinyl Label Material 3M™ Screen Printable Sheet Vinyl Label Materials 7200, 7902 and 7906 are durable, high performance materials that offer excellent conformability, good durability and moisture resistance. These mate.. |
|||
Peel Strength | 0.351 kN/m | 2.00 pli | 90° Peel, PET/Aluminum, Initial (20 mins); ASTM D3330 |
3M 9056MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |