Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.3287 kN/m | 1.875 pli | Composite Sleeve, Adhesion; ASTM D3330 |
3M 414DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Adhesion to Steel; ASTM D3330 |
3M 4195-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 4195-EZ is an easy unwind tapes coated with a very high-tack adhesive system to help provide temporary protection of automotive carpets, fabric interiors and carpe.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Composite Sleeve, Adhesion; ASTM D3330 |
3M 447DL Flexomount™ Solid Printing Tapes 3M™ Flexomount™ Solid Printing Tapes are double coated tapes designed for mounting photopolymer and rubber printing plates to flexographic printing cylinders or sleeve systems. The adhesive system.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Finely Textured Powder Coating, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7779 Polypropylene Label Material 3M™ Polypropylene Label Material 7779 with 3M™ Adhesive 350 can permanently bond to high surface energy (HSE) and low surface energy (LSE) plastics, textured and contoured surfaces, powder coating.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Adhesion to steel; ASTM D1000 |
3M CN-3490 EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Linered side-Rubber, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1020R Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ E1120 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Adhesion to Steel; ASTM D3330 |
3M 5193-EZ Polyethylene Protective Tapes 3M™ Polyethylene Protective Tapes 5193-EZ is an easy (EZ) unwind polyethylene tape with a very high-tack adhesive system.Information provided by 3M |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polypropylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | High Density Polyethylene, 180° Peel, initial 10 min dwell at RT; ASTM D3330 |
3M 7120 Performance Paper Label Material 3M™ Label Materials 7120 and 7122 latex impregnated paper with 3M™ 400 and 320 adhesives offer good conformability to curved surfaces and resistance to staining and moisture. Label Material 7120 h.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | HDPE, 180° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7604FP Primalyn™ White Vinyl Label Material 3M™ Primalyn™ White Vinyl Label Material 7604FP is a flexible vinyl providing excellent squeeze bottle performance with consistent printability. This material utilizes 3M™ Adhesive 300, which has.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polypropylene, 180° Peel, Conditioned for 3 days at RT; ASTM D3330 |
3M 7710 Acetate Identification Label Material 3M™ Label Material 7710 gloss clear acetate with 3M™ 400 high tack acrylic adhesive offers consistent, high quality appearance and excellent UV resistance. The transparent film easily die-cuts whi.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polypropylene, 180° Peel, Conditioned for 3 Days at RT; ASTM D3330 |
3M 7841 Laser Toner Printable Label Material 3M™ Label Material 7841 with 3M™ Adhesive 310 is designed for continuous laser printing offering good print contrast when bar coding and excellent toner anchorage. The Adhesive 310 resists oozing .. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polypropylene, 90° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7845TL Laser Toner Printable Polyester Label Material 3M™ Laser Toner Printable Polyester Label Material 7845TL is a matte clear polyester designed for sheet fed laser imprinting. This label material utilizes 3M™ Adhesive 310 which provides firmness .. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7881 Computer-Imprintable Polyester Label Material Features:Topcoated polyester is compatible with dot matrix printing and is hand writeable. The matte coating resists degradation from scuffing, chemicals, moisture, and wide temperature fluctuations.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7883 Computer-Imprintable Polyester Label Material 3M™ Dot Matrix Label Materials 7883 is a 3.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft liner.Features:Unique Top Coat for tradition.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7883HL Computer-Imprintable Polyester Label Material Information provided by 3M |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7893 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials 7980 and 7983 are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polypropylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7907 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Material 7907 is a durable, high performance material that offers excellent thermal stability, moisture resistance and chemical resistance. This label mat.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | LD Polyethylene, 90° Peel, Initial, 10 min dwell at RT; ASTM D3330 |
3M 7909 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | LD Polyethylene, 90° Peel, Conditioned for 24 hrs at 32°C at 90% RH; ASTM D3330 |
3M 7950 Screen Printable Sheet Polyester Label Material 3M™ Screen Printable Sheet Polyester Label Materials are durable, high performance materials that offer excellent thermal stability, moisture resistance and chemical resistance. These materials uti.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Polycarbonate 180° Peel, Conditioned for 3 days at 49°C; ASTM D3330 |
3M 7887 Computer-Imprintable Polyester Label Material 2.3 mil matte topcoated silver polyester facestock with 0.8 mil acrylic adhesive 300 on a 55 lb densified kraft linerFeatures:Unique Top Coat for traditional Dot Matrix printing, but delivers abrasi.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Non-linered side-Stainless Steel, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1120 Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Peel Strength | 0.3287 kN/m | 1.875 pli | Non-linered side-Urethane-B, Adhesion; ASTM D3330 |
3M Cushion-Mount™ 1915M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |