Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.10408 kN/m | 0.59375 pli | to Steel; ASTM D3330 |
3M Scotch® 4735 High Temperature Fine Line Tape Scotch® High Temperature Fine Line Tape 4735 is a vinyl fine line paint masking tape for fascia, rocker panels, two-tone and other multiple color applications where critical paint break lines are r.. |