Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 300 g/25 mm @Pressure 0.138 MPa, Temperature 115 °C |
300 g/in @Pressure 20.0 psi, Temperature 239 °F |
0.8 sec, Untreated; ExxonMobl Method |
ExxonMobil Bicor™ 15MB400 OPP Film Product Description: Bicor 15MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.138 MPa, Temperature 115 °C |
300 g/in @Pressure 20.0 psi, Temperature 239 °F |
EMS, 0.8 sec, Untreated; ExxonMobl Method |
ExxonMobil Bicor™ 20MB400 OPP Film Product Description: Bicor 20MB400 is a one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.138 MPa |
300 g/in @Pressure 20.0 psi |
0.8 sec; ExxonMobil Method |
ExxonMobil Oppalyte™ 38DO447 OPP Film Product Description: A super white opaque BOPP film. The Diamex technology allows for super low density and very high yield. Diamex makes it possible to lower the density, without decreasing the mod.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
300 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Oppalyte™ 38ICE OPP Film Product Description: A coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal .. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.138 MPa, Temperature 115 °C |
300 g/in @Pressure 20.0 psi, Temperature 239 °F |
0.8 sec, Untreated; ExxonMobl Method |
ExxonMobil Bicor™ 17MB400 OPP Film Product Description: Bicor 17MB400 is one side treated, sealable coextruded OPP film. It is designed for use in laminations.Availability: Africa & Middle East, Asia Pacific and EuropeKey Features:Ou.. |
|||
Seal Strength | 300 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
300 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Oppalyte™ 33ICE OPP Film Product Description: Coextruded white opaque, low density, biaxially oriented polypropylene film. This film is designed for the ice cream applications, and is suitable for heat seal and cold seal on.. |