Mechanical Properties Metric English Comments
Seal Strength 2400 g/25 mm
2400 g/in
Sentinel Sealer Test
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Seal Strength 2400 g/25 mm
2400 g/in
Sentinel Sealer Test
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e..
Seal Strength >= 2400 g/25 mm
>= 2400 g/in
Sentinel Sealer Test
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..
Seal Strength <= 2400 g/25 mm
<= 2400 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1702-1 Zinc Ionomer Resin for Extrusion Coating  (discontinued **)
Surlyn® 1702-1 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutic..
Seal Strength <= 2400 g/25 mm
<= 2400 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film
Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati..
Seal Strength >= 2400 g/25 mm
>= 2400 g/in
Sentinel Sealer Test
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness  (discontinued **)
Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st..