Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 4000 g/25 mm | 4000 g/in | F-88-68(73) |
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 150 Gauge
(discontinued **) Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc.. |
|||
Seal Strength | 4000 g/25 mm | 4000 g/in | HDPE, bar temp 150-175°C |
DuPont Appeel® LSR 1184 Modified EVA Lidding Sealing Resin
(discontinued **) Appeel® 1184 is an extrusion coatable resin designed to be a sealing layer for lidding applications. It provides peelable seals over a broad temperature range to a number of container materials inc.. |