Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 2400 g/25 mm | 2400 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Seal Strength | 2400 g/25 mm | 2400 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Seal Strength | >= 2400 g/25 mm | >= 2400 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Seal Strength | <= 2400 g/25 mm | <= 2400 g/in | Varies with seal bar temp. |
DuPont™ Surlyn® 1702-1 Zinc Ionomer Resin for Extrusion Coating
(discontinued **) Surlyn® 1702-1 is an ionomer resin available for use in conventional extrusion coating and coextrusion coating equipment designed to process polyethylene resins. Applications: Medical/pharmaceutic.. |
|||
Seal Strength | <= 2400 g/25 mm | <= 2400 g/in | Varies with seal bar temp. |
DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |
|||
Seal Strength | >= 2400 g/25 mm | >= 2400 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 76.2 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |