Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 2000 g/25 mm | 2000 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® LX-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.A linear low density polyethylene film with an outstanding combination of toughness and durability. LX has superior tensile strength, puncture strength, e.. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | seal bar 150°C. |
DuPont Nucrel® 30707SR Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating
(discontinued **) 7 wt% Acrylic Acid.Nucrel® 30707SR is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusio.. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | seal bar 150°C. |
DuPont Nucrel® 30707 Ethylene-Acrylic Acid Copolymer Resin for Film and Extrusion Coating 7 wt% Acrylic Acid.Nucrel® 30707 is an ethylene-acrylic acid copolymer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion .. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | Seal Bar Temp approx. 115-145°C |
DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | Seal Bar Temp approx. 120-145°C |
DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | Seal Bar Temp approx. 125-150°C |
DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |
|||
Seal Strength | 2000 g/25 mm | 2000 g/in | Seal Bar Temp approx. 140-150°C |
DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
Seal Strength | 2000 - 3400 g/25 mm | 2000 - 3400 g/in | Average value: 2530 g/25 mm Grade Count:21 |
Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Seal Strength | >= 2000 g/25 mm | >= 2000 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® SL-1 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |
|||
Seal Strength | >= 2000 g/25 mm | >= 2000 g/in | Sentinel Sealer Test |
DuPont™ Sclairfilm® SL-3 LLDPE Film, Laminating, 50.8 µm Thickness
(discontinued **) Data provided by DuPont Packaging Polymers.SL is a linear low density polyolefin film which offers a combination of toughness and durability plus outstanding clarity. These have superior tensile st.. |