Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 317 MPa | 46000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74836 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme Polyethylene SC74836 is a high strength linear low density polyethylene designed for blown film extrusion. This resin contains no slip, no antiblock and processing aid. Films.. |
|||
1% Secant Modulus, TD | 317 MPa | 46000 psi | ASTM D882 |
ExxonMobil Exceed™ 1327CA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327CA is a metallocene ethylene-hexene copolymers. It produces films which have high modulus whilst retaining good toughness. These properties together with excellent dr.. |
|||
1% Secant Modulus, TD | 317 MPa | 46000 psi | ASTM D882 |
ExxonMobil Exceed™ 1327ED Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327ED is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327ED is fully formula.. |
|||
1% Secant Modulus, TD | 317 MPa | 46000 psi | ASTM D882 |
ExxonMobil Exceed™ 1327KD Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 1327KD is a metallocene ethylene-hexene copolymer. It produces films which have high modulus whilst retaining good toughness. Additionally, Exceed 1327KD is fully formula.. |
|||
1% Secant Modulus, TD | 317 MPa | 46000 psi | ASTM D882 |
ExxonMobil LDPE LD 171BA Low Density Polyethylene Resin (European Grade) Product Description: LD 171BA is an LDPE grade, which offers good film rigidity combined with very good optical properties.Availability: Europe Additive: Antiblock: NoSlip: NoThermal Stabilizer: No.. |
|||
1% Secant Modulus, TD | 317 MPa | 46000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74859 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74859 polymer is a high strength linear low density polyethylene designed for blown film extrusion that contains no slip, high antiblock and high processing aid.Application/U.. |