Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
LyondellBasell Petrothene® NA336149 Low Density Polyethylene ApplicationsPETROTHENE NA 336 is a homopolymer resin specifically engineered for garment film and dry cleaning bag applications. This resin is also suitable for any application requiring thin gauge.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
LyondellBasell Petrothene® NA340141 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
LyondellBasell Petrothene® NA340163 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM E111 |
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM E111 |
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
LyondellBasell Petrothene® NA442051 Low Density Polyethylene ApplicationsPETROTHENE NA 442 is a series of low density/EVA copolymer resins for high impact/high clarity packaging and lamination applications. NA 442 exhibits excellent processability and good b.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
LyondellBasell Petrothene® NA340013 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
ExxonMobil LDPE LD 312.23 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
ExxonMobil LDPE LD 312.82 Low Density Polyethylene Resin Product Description: LD 312 resins are 4.6% vinyl acetate copolymers for films with good toughness. The comonomer content and low melt index of those resins help produce films which exhibit superior.. |
|||
1% Secant Modulus, TD | 165 MPa | 24000 psi | ASTM D882 |
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. .. |