Mechanical Properties Metric English Comments
1% Secant Modulus, TD 156.90 MPa
22757 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile..
1% Secant Modulus, TD 156.90 MPa
22757 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre..
1% Secant Modulus, TD 156.90 MPa
22757 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..
1% Secant Modulus, TD 156.90 MPa
22757 psi
ASTM D882
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin  (discontinued **)
Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt..