Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 290 MPa | 42100 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 are characterized by an.. |
|||
1% Secant Modulus, TD | 290 MPa | 42100 psi | ISO 527-3 |
Polimeri Europa Flexirene® FG 30 U Butene Copolymer Linear Low Density Polyethylene Flexirene FG 30 U is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Films manufactured with Flexirene FG 30 U are characterized b.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
Westlake LF2010 Hexene Linear Low Density Polyethylene Westlake LF2010 is a hexene LLDPE with increased stiffness suitable for heavy duty films and shipping sacks. This material contains process aid for improved ease of extrusion, and can be blended wit.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil LD 071.LQ Blown Film Resin L Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tou.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil LD 071.LR Blown Film Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LQ Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil LDPE LD 071.LR Low Density Polyethylene Resin Product Description: LD 071 Series case wrap film resins combine good processability with excellent strength and good film optics for bundling applications requiring proper shrink performance, tough.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil LDPE LD 156BW Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |
|||
1% Secant Modulus, TD | 290 MPa | 42000 psi | ASTM D882 |
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |