Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 1720 MPa | 250000 psi | ASTM D882 |
ExxonMobil HDPE HTA 108 High Density Polyethylene Resin Product Description: HTA 108 is a homopolymer HDPE film grade designed to improve stiffness and barrier in coextrusion or in PE blends. When blended with LLDPE, HTA 108 improves their processability.. |