Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
LyondellBasell Petrothene® NA334000 Low Density Polyethylene ApplicationsPETROTHENE NA 334-000 is a homopolymer resin specifically engineered for thin film applications. NA 334-000 is know for its consistency, exceptional drawdown and processability. Regulat.. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
LyondellBasell Petrothene® NA350136 Low Density Polyethylene ApplicationsPETROTHENE NA 350-136 is a low density/EVA copolymer designed for heavy duty film packaging and other high strength, easy to seal packaging. NA 350-136 exhibits high impact strength and.. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480145 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480177 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
LyondellBasell Petrothene® NA480178 Low Density Polyethylene ApplicationsPETROTHENE NA 480 is a series of low density/EVA copolymer resins designed for specialty films. NA 480 produces film with superior puncture resistance, Heat sealability, clarity and low.. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74840 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74840 linear low density polyethylene is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more c.. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
Westlake Mxsite LC78104 Polyethylene Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling .. |
|||
1% Secant Modulus, TD | 159 MPa | 23000 psi | ASTM D882 |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |