Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 156.90 MPa | 22757 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL1061 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1061 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant, antiblock and slip agent. Films made from Titanceed® mL1061 have outstanding tensile.. |
|||
1% Secant Modulus, TD | 156.90 MPa | 22757 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL1064 Linear low density polyethylene resin
(discontinued **) Titanceed® mL1064 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. Films made from Titanceed® mL1064 have outstanding tensile, impact and puncture stre.. |
|||
1% Secant Modulus, TD | 156.90 MPa | 22757 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL156 Linear low density polyethylene resin
(discontinued **) Titanceed® mL156 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |
|||
1% Secant Modulus, TD | 156.90 MPa | 22757 psi | ASTM D882 |
Lotte Chemical Titan TITANCEED® mL216 Linear low density polyethylene resin
(discontinued **) Titanceed® mL216 is a pelleted metallocene linear low density polyethylene resin formulated with antioxidant. This product is used for blown film extrusion which offers outstanding tensile strengt.. |