Mechanical Properties Metric English Comments
1% Secant Modulus, TD 1370 MPa

@Thickness 0.0254 mm
199000 psi

@Thickness 0.00100 in
ASTM D882A
Total 9458 HDPE Film Grade
Medium molecular weight grade. Excellent bubble stability, good compatibility with LDPE and LLDPE, good heat resistance, high stiffness and tensile strength.Applications: Release liners, Stand-up ba..