Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 1030 MPa | 150000 psi | ASTM D822 |
LyondellBasell Alathon® M6060 High Density Polyethylene ApplicationsALATHON M 6060 is a medium molecular weight high density homopolymer with extremely low gel content. This resin provides high stiffness and narrow molecular weight distribution for use .. |