Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 67.6 MPa | 9810 psi | ASTM D882 |
ExxonMobil ESCOR™ AT 310 Blown Film Resin
(discontinued **) ESCOR AT 310 is an acid terpolymer which provides excellent adhesion to a variety of polar and non-polar materials such as metals, glass, polyolefins, polyamides, polyesters, etc. It is suitable fo.. |