Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 60.0 MPa | 8700 psi | ASTM D882 |
SABIC HP4023W Low Density Polyethylene for Blown Film Product Description: HP4023W is a Low Density Polyethylene grade suitable for producing general purpose films and contains slip and antiblock additives. It yields excellent processability with goo.. |
|||
1% Secant Modulus, MD | 60.0 MPa | 8700 psi | ASTM D882 |