Mechanical Properties Metric English Comments
1% Secant Modulus, MD 490 MPa
71100 psi
ASTM-D882
Braskem FH35 HDPE Cast Film Extrusion Polyethylene Copolymer
The FH35 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process for flat die film extrusion with good mechanical properties. It contains antioxidant additives...