Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 169 MPa
24500 psi
ASTM D882
ExxonMobil Exceed™ 2018CA Blown Film Resin  (discontinued **)
Exceed 2018CA resin is an ethylene based polymer produced with metallocene single site catalysts using ExxonMobil Chemicals EXXPOL® Technology. The higher melt index makes this polymer ideally sui..