Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Riblene® FC 30 Low Density Polyethylene - Blown Film Extrusion Riblene FC 30 is a high molecular weight low density polyethylene resin (LDPE) suitable for blown film extrusion. Riblene FC 30 is characterized by a high melt strength leading to a good bubble sta.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 20 Low Density Polyethylene - Blown Film Extrusion Riblene FF 20 is a high molecular weight low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FF 20 is characterized by a good melt strength leading to a good bubble stability.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Riblene® FF 29 Low Density Polyethylene - Blown Film Extrusion Riblene FF 29 is a high molecular weight low density polyethylene (LDPE), suitable for blown film extrusion. Riblene FF 29 is characterized by a good melt strength leading to a good bubble stabilit.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion Riblene FH 10 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FH 10 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Riblene® FL 20 Low Density Polyethylene - Blown Film Extrusion Riblene FL 20 is a low density polyethylene (LDPE) suitable for blown film extrusion. Riblene FL 20 is characterized by a good balance between processability and mechanical properties.Films manufac.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Riblene® FM 23 Low Density Polyethylene - Blown Film Extrusion Riblene FM 23 is a low density polyethylene (LDPE) with added slip and antiblocking agents, suitable for blown film extrusion. Riblene FM 23 is characterized by a good balance between processabilit.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ASTM D 882 |
NOVA Chemicals Surpass® FPs225-A Octene Copolymer sLLDPE Film Resin FPs225-A complies with the U.S. FDA regulations for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without .. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LGH 138 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 138 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, slip agent, antiblocking and processing aid, suitable for blown film extrusion.Films obtai.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ASTM-D882 |
Braskem FG31 LLDPE Blown Film Extrusion Polyethylene Copolymer FG31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for blown film extrusion in blends with polyethylene. Films obtained with this pr.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ASTM-D882 |
Braskem LL6901S LLDPE Blown Film Extrusion Polyethylene Copolymer LL6901S is a LLDPE Butene copolymer produced by Braskem. It is a ready to use product since it's been compounded with 15% LDPE. It is a general purpose product that shows a good processing performan.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T LGH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T LGH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films obtained from Clearflex H&T LGH.. |
|||
1% Secant Modulus, MD | 160 MPa | 23200 psi | ASTM D882 |
SABIC HP2022 Series Low Density Polyethylene for Blown Film Product Description: HP2022 series resins are Low Density Polyethylene grades suitable for general purpose packaging. They exhibit better draw down, good optical and mechanical properties.HP2022N:.. |