Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 145 MPa | 21000 psi | ISO 527-3 |
Polimeri Europa Clearflex® H&T CMH 108 Octene Copolymer Linear Low Density Polyethylene Clearflex H&T CMH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CMH 108 show e.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LD 135.09 Cast Packaging Film Resin
(discontinued **) LD 135.09 is a homopolymer film resin with good clarity. It is suitable for processing in cast film equipment. Applications include food packaging, light to medium duty bags, and textile packaging.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
Westlake EF444 4.7% Ethylene Vinyl Acetate Copolymer
(discontinued **) Excellent haze and gloss, excellent impact strength and very good sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, section 177.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
LyondellBasell Petrothene® NA340141 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
LyondellBasell Petrothene® NA340163 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM E111 |
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM E111 |
LyondellBasell Petrothene® NA340212 Low Density Polyethylene, Film Extrusion Grade PETROTHENE NA340 is a series of LDPE/EVA copolymer resins designed for quality bags and special film applications that require clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
LyondellBasell Petrothene® NA340013 Low Density Polyethylene ApplicationsPETROTHENE NA 340 is a LDPE/EVA copolymer resin designed for quality bags and special film applications requiring clarity and excellent impact strength. Typical applications include hea.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
Westlake Elevate™ EF439 4.0% Ethylene Vinyl Acetate Copolymer Excellent haze and gloss, excellent impact strength and very good heat sealability.Application/UsesHigh clarity packagingHigh impactFDA: This material complies with FDA regulations in 21 CFR, sectio.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. .. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.32 Low Density Polyethylene Resin (European Grade) Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high clarity film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impa.. |
|||
1% Secant Modulus, MD | 145 MPa | 21000 psi | ASTM D882 |
ExxonMobil LDPE LD 302.56 Low Density Polyethylene Resin Product Description: LD 302 resins are 3.5% vinyl acetate copolymer, high film resins. The combination of comonomer content and low melt index helps produce films which exhibit superior impact stren.. |