Polymer Property : 1% Secant Modulus, MD = 20300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Clearflex® H&T CLH 108 Octene Copolymer Linear Low Density Polyethylene
Clearflex H&T CLH 108 is an octene copolymer linear low density polyethylene (C8-LLDPE), with antioxidants, suitable for cast film extrusion. Stretch films obtained from Clearflex H&T CLH 108 show e..
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Flexirene® FG 20 F Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 20 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 F is recommended for the ..
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Flexirene® FG 23 I Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 23 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 I represents the version of Flexirene FG 20 I..
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Greenflex® FL 25 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion
Greenflex FL 25 is an ethylene vinyl acetate copolymer (EVA) for blown film extrusion. Films produced with Greenflex FL 25 show good optical properties and excellent sealability.Main Applications: ..
1% Secant Modulus, MD 140 MPa
20300 psi
ASTM D 882
NOVA Chemicals Sclair® FP019-C Octene Copolymer LLDPE Film Resin
FP019-C is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Polymer Process AidApplications: High toughness film,..
1% Secant Modulus, MD 140 MPa
20300 psi
ASTM D 882
NOVA Chemicals Sclair® FP019-D Octene Copolymer LLDPE Film Resin
FP019-D is biologically and chemically inert.Features: Superior toughness, Outstanding melt strength, Excellent sealability, Low gelAdditives: Slip, Antiblock, Polymer Process AidApplications: Hig..
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Flexirene® FG 20 I Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 20 I is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Main Applications: Flexirene FG 20 I is recommended for the ..
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Flexirene® FG 23 F Butene Copolymer Linear Low Density Polyethylene
Flexirene FG 23 F is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.Flexirene FG 23 F represents the version of Flexirene FG 20 F..
1% Secant Modulus, MD 140 MPa
20300 psi
ASTM-D882
Braskem FL31 LLDPE Cast Film Extrusion Polyethylene Copolymer
FL31 is a linear low-density polyethylene, copolymer of butene-1, produced by the solution process. It was developed for cast film extrusion. Films obtained with this product show a good processing ..
1% Secant Modulus, MD 140 MPa
20300 psi
ISO 527-3
Polimeri Europa Clearflex® H&T CLH 196 Hexene Copolymer Linear Low Density Polyethylene
Clearflex H&T CLH 196 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Stretch films manufactured with Clearflex H&T CLH 196 have..