Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 841 MPa | 122000 psi | ASTM D882 |
Chevron Phillips MarFlex® 9656 HDPE Blown Film Resin Resin Type: high density, linear polyethylene.Characteristics: copolymerization enhances film toughness, good drawdown, density level gives good machinability, blend well with LLDPEApplications: not.. |