Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 827 MPa | 120000 psi | ASTM D822 |
LyondellBasell Alathon® L5845 High Density Polyethylene ApplicationsALATHON L 5845 is a medium molecular weight high density homopolymer for use in blown film applications. Typical applications include paper replacement, coextrusions and laminations.Reg.. |
|||
1% Secant Modulus, MD | 827 MPa | 120000 psi | ASTM D822 |
LyondellBasell Alathon® M6020 High Density Polyethylene ApplicationsALATHON 6020 is a medium molecular high density weight homopolymer for use in blown or cast film applications. This resin provides extremely low gel content and high stiffness. Typica.. |