Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 793 MPa | 115000 psi | ASTM D822 |
LyondellBasell Alathon® M6060 High Density Polyethylene ApplicationsALATHON M 6060 is a medium molecular weight high density homopolymer with extremely low gel content. This resin provides high stiffness and narrow molecular weight distribution for use .. |
|||
1% Secant Modulus, MD | 793 MPa | 115000 psi | ASTM D822 |
LyondellBasell Alathon® L5005 High Density Polyethylene ApplicationsALATHON L 5005 is a high molecular weight high density copolymer that provides broad bimodal molecular weight distribution, high stiffness and good heat seal response and strength. Typi.. |