Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 51.0 MPa | 7400 psi | ASTM D882 |
ExxonMobil Escorene™ FL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: FL 00018 is a copolymer of ethylene and vinyl acetate. It offers combines toughness, good optical and sealing properties and low gel. In particular, its good behavior in high fr.. |
|||
1% Secant Modulus, MD | 51.0 MPa | 7400 psi | ASTM D882 |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
1% Secant Modulus, MD | 51.0 MPa | 7400 psi | ASTM D882 |
ExxonMobil Escorene™ UL 00018 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00018 is a fractional MI copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Applic.. |
|||
1% Secant Modulus, MD | 51.0 MPa | 7400 psi | ASTM D882 |
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It can produce f.. |