Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 365 MPa | 52900 psi | 2.5 BUR; ASTM D882 |
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica.. |
|||
1% Secant Modulus, MD | 365 MPa | 52900 psi | 4 BUR; ASTM D882 |
Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film This LDLPE is tailored for applications that require:Good processabilityGood melt strengthGood drawdownGood strengthSatin finishGood MD & TD shrinkageGood contact clarity and lower gel contentTypica.. |
|||
1% Secant Modulus, MD | 365 MPa | 53000 psi | ASTM D882, A |
Total Lumicene® mPE M 3410 EP Metallocene Medium Density Film Resin
(Unverified Data**) Polyethylene: Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityHigh StiffnessGood puncture resistanceGood tear strengthGood heat sealing p.. |