Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
LyondellBasell Petrothene® GA601031 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
LyondellBasell Petrothene® GA601032 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
LyondellBasell Petrothene® GA601033 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
LyondellBasell Petrothene® GA601030 Linear Low Density Polyethylene ApplicationsPETROTHENE® GA 601 series are pelletized, linear low density polyethylenes for applications requiring maximum strength and toughness. These products offer excellent additive homogene.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
Westlake EF418 Low Density Polyethylene WESTLAKE polyethylene EF418 is a LDPE formula with excellent optical properties suggested by light and medium duty packaging.Application/UsesLight and medium duty produce bagsClarity packagingGenera.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
Westlake EN1817AA Low Density Polyethylene Westlake Polyethylene EN1817 is a low density formulation suggested for film applications requiring high clarity, good tear and impact strength, good printability and a wide heat-sealing range.Appli.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
Westlake EN1820 Low Density Polyethylene Westlake Polyethylene EN1820 natural is a low density formulation with outstanding optical properties, making this material an excellent choice for calendaring and as a clarity filler in coextruded .. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
Westlake LF2020 Hexene Linear Low Density Polyethylene Westlake LF2020 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10CB Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10HA Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil Enable™ 20-10HE Metallocene Polyethylene Resin Product Description: Enable 20-10 resins are metallocene ethylene-hexane copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact .. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 165BW1 Low Density Polyethylene Resin (European Grade) Product Description: LD 165 series are LDPE grades, offering high strength combined with medium optical properties.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: NoTherm.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
1% Secant Modulus, MD | 207 MPa | 30000 psi | ASTM D882 |
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |