Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
NOVA Chemicals Novapol® LA-0219-A LDPE Foam Resin Features: Good heat sealing latitudeModerate toughnessEasy processability Applications: Industrial packagingLinersBlends with LLDPEFoam ArticlesInformation provided by Nova Chemicals |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
ExxonMobil LD 145.PX Packaging Resin
(discontinued **) LD 145.PX resin is a homopolymer cast film resin offering good clarity and toughness. Applications include Bread bags and other Food Packaging.Information provided by ExxonMobil Chemical |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake EF601 Low Density Polyethylene Westlake EF601 is a fractional melt LDPE with excellent toughness. It is suggested in heavy duty films and shipping sacks, and in industrial shrink applications. It can be used as a bubble stabilize.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake EF603 Low Density Polyethylene Westlake EF603 is a LDPE resin with excellent toughness and processability. It is suggested in heavy duty films and medium duty shrink applications. It can be used as a bubble stabilizer in LLDPE ri.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake EF606 Low Density Polyethylene Westlake EF606 is a LDPE resin suggested for use in multiwall and general purpose liners, and for use as a blend resin in general purpose packaging applications. It has excellent processability, and.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake EF608 Low Density Polyethylene Westlake EF608 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake Hifor Xtreme SC74840 Linear Low Density Polyethylene WESTLAKE HIFOR Xtreme SC74840 linear low density polyethylene is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more c.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake Mxsite LC78104 Polyethylene Mxsite LC78104 polyethylene is recommended for the skin layers of cast stretch film. It will provide a very aggressive cling force in both a stretched and unstretched condition. The excellent cling .. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
Westlake Mxsten CV77518 Polyethylene Plastomer Mxsten CV Plastomer CV77518 resin is a polyethylene plastomer designed for blown and cast film extrusion that contains no slip and no antiblock additives. Films produced with this resin exhibit a ve.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
ExxonMobil LD 141.87 Shrink Film Resin LD 141.87 is a vinyl acetate copolymer film resin with very good toughness and shrink properties. Applications include Medium duty shrink wrap and Heavy duty bags.Information provided by ExxonMobil.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
ExxonMobil LDPE LD 313.NF Low Density Polyethylene Resin Product Description: LD 313.NF is a 3 % vinyl acetate copolymer. The vinyl acetate content of this resin provides good heat sealing and good cold temperature toughness when compared to LDPE homopoly.. |
|||
1% Secant Modulus, MD | 152 MPa | 22000 psi | ASTM D882 |
ExxonMobil LDPE LD 358BW Low Density Polyethylene Resin (European Grade) Product Description: LD 358BW is an EVA LDPE which offers a combination of excellent sealability and toughness even at low temperatures.Availability: Europe Additive: Antiblock: NoSlip: No Thermal .. |