Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Yield Strength = 252 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 252 MPa
36500 psi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP OCL36AXP PPS (Europe-Africa-Middle East)
LNP* LUBRICOMP* OCL36AXP is a compound based on PPS-Branched resin containing Carbon Fiber, PTFE. Added features include: Electrically Conductive, Internally Lubricated.
Flexural Yield Strength 252 MPa
36500 psi
ASTM D790
Chem Polymer Chemlon 240 G Nylon 6, 43% Glass Fiber Reinforced
A 43% glass fiber reinforced nylon 6, offering high rigidity and tensile strength, especially at high service temperatures.Data provided by the manufacturer, Chem Polymer.
Copyright © lookpolymers.com All Rights Reserved