Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 75.0 - 455 MPa | 10900 - 66000 psi | Average value: 275 MPa Grade Count:245 |
Overview of materials for Nylon 66, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. .. |