Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 120.658 - 365 MPa @Temperature 115 - 150 °C |
17500.0 - 52900 psi @Temperature 239 - 302 °F |
Average value: 243 MPa Grade Count:2 |
Overview of materials for Vinyl Ester Sheet Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Vinyl Ester Sheet Molding Compound". Each property range of values reported is minimum and maximum value.. |