Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 66.2 - 297 MPa | 9600 - 43100 psi | Average value: 234 MPa Grade Count:23 |
Overview of materials for Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 30% Carbon Fiber Filler". Specific grades with carbon fiber content bet.. |