Polymer Property : Flexural Yield Strength = 29700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Yield Strength 59.0 - 205 MPa
8560 - 29700 psi
Average value: 112 MPa Grade Count:11
Overview of materials for Nylon 6, Mineral Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Mineral Reinforced, Impact Grade". Each property range of values reported is minimum and maximu..
Flexural Yield Strength 27.6 - 205 MPa
4000 - 29700 psi
Average value: 90.5 MPa Grade Count:340
Overview of materials for Polycarbonate, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Molded". Each property range of values reported is minimum and maximum values of appropri..