Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 48.3 - 2000 MPa | 7000 - 290000 psi | Average value: 300 MPa Grade Count:182 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Flexural Yield Strength | 110 - 2000 MPa | 16000 - 290000 psi | Average value: 915 MPa Grade Count:32 |