Mechanical Properties Metric English Comments
Flexural Yield Strength 70.0 - 186 MPa
10200 - 27000 psi
Average value: 123 MPa Grade Count:31
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Flexural Yield Strength 138 - 186 MPa
20000 - 27000 psi
Average value: 165 MPa Grade Count:8
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 30% Carbon Fiber Filled". Specific grades with carbon fiber conte..
Flexural Yield Strength 86.0 - 186 MPa
12500 - 27000 psi
Average value: 95.9 MPa Grade Count:14
Overview of materials for Polycarbonate, High Heat
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, High Heat". Each property range of values reported is minimum and maximum values of appro..
Flexural Yield Strength 82.7 - 186 MPa
12000 - 27000 psi
Average value: 111 MPa Grade Count:115
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Flexural Yield Strength 17.2 - 186 MPa
2500 - 27000 psi
Average value: 71.9 MPa Grade Count:52
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum..
Flexural Yield Strength 36.5 - 186 MPa
5300 - 27000 psi
Average value: 77.2 MPa Grade Count:99
Overview of materials for Acetal Copolymer, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, PTFE Filled". Each property range of values reported is minimum and maximum values of ..
Flexural Yield Strength 82.7 - 186 MPa
12000 - 27000 psi
Average value: 121 MPa Grade Count:11
Overview of materials for Acrylic/Polycarbonate Alloy, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy, Glass Fiber Filler". Each property range of values reported is minimum and ..
Flexural Yield Strength 55.0 - 186 MPa
7980 - 27000 psi
Average value: 101 MPa Grade Count:26
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Flexural Yield Strength 31.0 - 186 MPa
4500 - 27000 psi
Average value: 75.4 MPa Grade Count:18
Overview of materials for Polypropylene, Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Carbon Fiber 10%". Each property range of values reported is minimum and maximum values o..