Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 96.0 - 181 MPa @Temperature 100 - 200 °C |
13900 - 26300 psi @Temperature 212 - 392 °F |
Average value: 119 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Flexural Yield Strength | 96.0 - 181 MPa @Strain 3.50 - 5.00 % |
13900 - 26300 psi @Strain 3.50 - 5.00 % |
Average value: 119 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Flexural Yield Strength | 68.9 - 181 MPa | 10000 - 26300 psi | Average value: 104 MPa Grade Count:28 |
Overview of materials for Acetal Copolymer, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Mineral Filled". Each property range of values reported is minimum and maximum values .. |
|||
Flexural Yield Strength | 181 - 181 MPa @Temperature 232 - 232 °C |
26300 - 26300 psi @Temperature 450 - 450 °F |
Average value: 181 MPa Grade Count:1 |
Overview of materials for Polyamide-Imide, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Glass Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 96.0 - 181 MPa @Temperature 100 - 200 °C |
13900 - 26300 psi @Temperature 212 - 392 °F |
Average value: 154 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Flexural Yield Strength | 96.0 - 181 MPa @Strain 3.50 - 5.00 % |
13900 - 26300 psi @Strain 3.50 - 5.00 % |
Average value: 154 MPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), Glass Fiber 40% This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Glass Fiber 40%". Specific grades with glass content between 35% and 44% are included. .. |
|||
Flexural Yield Strength | 13.4 - 181 MPa | 1950 - 26300 psi | Average value: 47.7 MPa Grade Count:128 |
Overview of materials for Polypropylene Copolymer This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp.. |