Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 13.0 - 179 MPa | 1890 - 26000 psi | Average value: 78.4 MPa Grade Count:230 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 68.9 - 179 MPa | 10000 - 26000 psi | Average value: 91.2 MPa Grade Count:63 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
Flexural Yield Strength | 84.1 - 179 MPa | 12200 - 26000 psi | Average value: 120 MPa Grade Count:21 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Flexural Yield Strength | 124 - 179 MPa | 18000 - 26000 psi | Average value: 145 MPa Grade Count:3 |
Overview of materials for Nylon 11 with 30% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ.. |
|||
Flexural Yield Strength | 72.4 - 179 MPa | 10500 - 26000 psi | Average value: 120 MPa Grade Count:20 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend, Glass Reinforced". Each property range of values repo.. |
|||
Flexural Yield Strength | 55.0 - 179 MPa | 7980 - 26000 psi | Average value: 128 MPa Grade Count:37 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Flexural Yield Strength | 110 - 179 MPa | 16000 - 26000 psi | Average value: 143 MPa Grade Count:4 |
Overview of materials for Acrylic, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values o.. |
|||
Flexural Yield Strength | 138 - 179 MPa | 20000 - 26000 psi | ASTM D790 |
Premix Premi-Glas® 1200-28 Polyester SMC
(discontinued **) Premi-Glas® 1200-28 series is a low profile, 28 % glass reinforced polyester Sheet Molding Compound designed for recreational vehicle body panels applications that require excellent flexibility and.. |