Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 68.9 - 147 MPa | 10000 - 21300 psi | Average value: 109 MPa Grade Count:35 |
Overview of materials for Acetal Copolymer, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% ar.. |
|||
Flexural Yield Strength | 100 - 147 MPa | 14500 - 21300 psi | Average value: 128 MPa Grade Count:8 |
Overview of materials for Epoxy, Molded, Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Mineral Filled". Each property range of values reported is minimum and maximum values of .. |