Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Yield Strength | 45.6 - 142 MPa | 6610 - 20600 psi | Average value: 73.4 MPa Grade Count:87 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Heat Resistant, Molded". Each property range of values reported i.. |
|||
Flexural Yield Strength | 65.5 - 142 MPa | 9500 - 20600 psi | Average value: 104 MPa Grade Count:65 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Flexural Yield Strength | 38.0 - 142 MPa | 5510 - 20600 psi | Average value: 92.7 MPa Grade Count:29 |
Overview of materials for Acrylic, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Extruded". Each property range of values reported is minimum and maximum values of appropriate .. |